AMMT-042 Pickup Abrasion-Resistant Material

AMMT-042 pickup abrasion-resistant material is the third-generation polyurea elastomer formed through on-site spraying of such raw materials as quasi-prepolymer, amine-terminated polyether and amine chain extender. As the revolutionary leap of the traditional construction technique, that technique organically combines the new materials, equipment and technologies, which is one of the most advanced construction techniques.
Product Details

Product introduction:


AMMT-042 pickup abrasion-resistant material is the third-generation polyurea elastomer formed through on-site spraying of such raw materials as quasi-prepolymer, amine-terminated polyether and amine chain extender. As the revolutionary leap of the traditional construction technique, that technique organically combines the new materials, equipment and technologies, which is one of the most advanced construction techniques.


Features:


★  Good abrasion resistance.

★  No joint, the surface is the uniform "pit" structure and is elegant.

★  Excellent weather fastness and chemical resistance.

★  With fast reaction speed and high production efficiency, it can be put into use soon.

★  Not sensitive to moisture or temperature, with good thermal stability.

★  Good physical performance, good adhesive force.

★  100% solid content without VOC and pollution.


Application:


AMMT-042 pickup abrasion-resistant material, with function of good abrasion resistance, anticorrosion, protection and decoration, is designed for truck, widely used for lining of light pickup, military truck, container car and lift truck.


Main performance indexes:


Solid content

100%

Gel time

10 seconds

Tensile strength

15Mpa

Elongation at break

200%

Tear strength

71KN/m

Hardness, Shao A

85~95

Adhesive force

11.8MPa

Abrasion resistance (Akron method)

4.9mg

Shock resistance

1.5kg.m

Electrical strength

20Mv/m

Water resistance (30d)

No rust, no bubble, no falling-off

Liquid medium resistant

No rust, no bubble, no falling-off

Salt fog resistance (2,000h)

No rust, no bubble, no falling-off

Artificial climate aging (2,000h)

Good

Low temperature flexibility (-30℃)

No crack

Density

1.02g/cm3 


All the parameters above are the physical performance tested after 7-day curing under the conditions of 23±2℃ and 50%±5% relative humidity after the spraying by Graco H-XP3 host &Fusion AP spray gun under laboratory condition.

Drying time (25℃)  The surface will be dry within 15 seconds, and it will reach the walk intensity within 10 minutes.

Thickness: 1-2mm (depending on user requirements)

Painting interval: Minimum: no time limit; Maximum: not more than 3 hours.


Substrate treatment:


Well compatible with current general automobile electrophoresis primer, and it can spray on the surface if the substrate surface is clean without grease and dust.


Coating method:


The high-temperature and high-pressure impact mixing equipment specified by our company must be used during construction. The loss caused by using the equipment not verified to be feasible by our company for the construction is at your own risk.


Packaging specifications:


Material A: 220kg/barrel; Material R: 200kg/barrel. The packaging can be changed in accordance with user requirement.


Storage and transportation: 


This product shall be stored in the shady and cool, ventilated and dry warehouse, and rain, sun and fire source shall be strictly prohibited, while it shall be far away from the heat source, and the storage temperature shall be 15-40℃.

Under the condition of not opening the original packaging, the storage period of the product is 6 months since the production date, and if it exceeds the storage period, conduct inspection for the items specified by the product standard, and the product can still be used if it meets the technical requirements.

The product doesn't contain organic solvent, so it can be transported as non-dangerous goods. The transportation shall be strictly prevented from rain and sun, and shall conform to the relevant regulations of the transport department.


Labor protection measures: 


When using the product, it is required to wear labor protection appliances like work clothes, goggles, gloves and gas mask.


Precautions: 


· During the construction, the substrate temperature shall be at least 3℃ higher than the dew point.

·  Fully stir component R until it is completely even before the construction.

·  The unfinished coating material of component A shall be sealed after filling nitrogen.

·  That system is 100% solid content, and the addition of any diluent is forbidden.

·  Good ventilation shall be guaranteed during the construction in a confined space.

Message
Submit